    Thermal shock behaviour of a kaolinte refractory prepared using a natural organic binder

    Thumbnail
    View/Open
    Fulltext (616.5Kb)
    Date
    2006
    Author
    Ogacho, AA
    Aduda, Bernard O
    Nyongesa, FW
    Type
    Article
    Language
    en
    Metadata
    Show full item record

    Abstract
    The thermal shock resistance of a kaolinite-based refractory prepared with a binder derived from a plant (corchorus olitorius) was investigated. Thermal shock tests employing water-quenching technique were performed at quench temperature differences of between 80 and 580 °C and then the damage parameter, and thermal shock parameters (R, R′, and R′′′) evaluated using measured strength and modulus values. The results showed that R and R′ parameters increased with increasing binder concentrations, an indication that the damage due to crack initiation was progressively impaired with increased binder concentrations. The R′′′ parameter on the other hand decreased with increasing binder concentrations indicating poor resistance of the material to crack propagation. These observations were also matched with thermal shock results which showed that samples plasticized with higher binder concentration had relatively very high strengths before thermal shock, compared to those plasticized with plain water, but they experienced rather large strength losses (over 60% of their initial values) at quench temperature difference (ΔT) exceeding 325 °C. The critical temperature difference (ΔT C) for the samples tested was in the range 250–325 °C. Scanning electron microscope (SEM) micrographs of samples quenched at temperature difference of 580 °C showed that samples plasticized with high binder concentration (0.68) experienced severe cracking of the matrix compared to their counterparts plasticized with plain water, whose microstructures showed an inhibited crack propagation.
    URI
    http://link.springer.com/article/10.1007/s10853-006-1007-6
    http://erepository.uonbi.ac.ke:8080/xmlui/handle/123456789/36820
    Citation
    Journal of Materials Science December 2006, Volume 41, Issue 24, pp 8276-8283
    Publisher
    Springer
     
    Department of Physics, University of Nairobi
     
    Collections
    • Faculty of Science & Technology (FST) [4284]

    Copyright © 2022 
    University of Nairobi Library
    Contact Us | Send Feedback

     

     

    Useful Links
    UON HomeLibrary HomeKLISC

    Browse

    All of UoN Digital RepositoryCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    LoginRegister

    Copyright © 2022 
    University of Nairobi Library
    Contact Us | Send Feedback